What are the common problems when using akd polymer emulsifier and how to solve them?

Sep 16, 2025

Leave a message

Hey there! As a supplier of AKD polymer emulsifier, I've seen my fair share of issues that customers run into when using this product. AKD, or alkyl ketene dimer, is a popular sizing agent in the papermaking industry. It helps improve the paper's resistance to water and other liquids. But like any product, it comes with its own set of common problems. In this blog, I'll walk you through those issues and share some tips on how to solve them.

1. Poor Sizing Efficiency

One of the most common problems is poor sizing efficiency. You might expect your paper to have a good level of water resistance after adding AKD polymer emulsifier, but it just doesn't live up to the mark. There could be several reasons for this.

First off, the dosage might be wrong. If you're not using enough AKD, the paper won't get properly sized. On the other hand, using too much can also be a problem. It can lead to an imbalance in the system and cause other issues like foam formation. To solve this, you need to do some testing. Start with the recommended dosage provided by us and then make small adjustments based on the results. You can also use some tools to measure the sizing degree of the paper, like the Cobb test.

Another factor that can affect sizing efficiency is the pH of the papermaking system. AKD works best in a slightly alkaline environment. If the pH is too low, the AKD might not react properly with the cellulose fibers in the paper. So, make sure to monitor and adjust the pH regularly. You can use pH meters to keep an eye on it and add pH adjusters if necessary.

2. Foam Formation

Foam is another headache when using AKD polymer emulsifier. Foam can cause all sorts of problems in the papermaking process. It can make it difficult to control the paper machine, lead to uneven paper formation, and even reduce the efficiency of the AKD itself.

The main reason for foam formation is usually the presence of surfactants or other chemicals in the system. Sometimes, these chemicals can interact with the AKD and create a foamy mess. To deal with this, you can use antifoaming agents. There are different types of antifoaming agents available, and you need to choose the one that's compatible with your papermaking system. You can also try to reduce the amount of other chemicals that might be causing the foam. For example, if you're using a Anionic Trash Catcher, make sure you're using the right dosage.

3. Deposit Formation

Deposit formation is yet another common problem. Over time, AKD and other substances can build up on the paper machine surfaces, like the wires and felts. These deposits can affect the quality of the paper and even damage the equipment.

The cause of deposit formation can be the reaction between AKD and other chemicals in the system, as well as the presence of impurities in the water or raw materials. To prevent deposit formation, you need to keep the papermaking system clean. Regularly clean the wires and felts using appropriate cleaning agents. You can also add some chemicals that can prevent the deposition, like dispersants. These chemicals can help keep the AKD and other substances in suspension and prevent them from sticking to the surfaces.

4. Compatibility Issues

Sometimes, AKD polymer emulsifier might not be compatible with other additives in the papermaking process. For example, if you're using a Cationic Retention and Drainage Aid along with AKD, there could be some interactions between them. This can lead to reduced performance of both products.

To solve this problem, you need to do some compatibility testing before using the products together. You can mix small amounts of the AKD and the other additive in a test sample and observe the results. If there are any signs of incompatibility, like precipitation or changes in viscosity, you might need to adjust the dosage or choose a different additive.

5. Storage and Handling Problems

Proper storage and handling of AKD polymer emulsifier are crucial. If it's not stored correctly, it can lose its effectiveness. AKD should be stored in a cool, dry place away from direct sunlight. High temperatures can cause the emulsion to break down, and moisture can also affect its quality.

When handling AKD, make sure to follow the safety instructions. It's important to wear appropriate protective equipment, like gloves and goggles, to avoid any contact with the skin or eyes. Also, make sure to mix the AKD properly before using it. Inadequate mixing can lead to uneven sizing and other problems.

6. Uneven Sizing

Uneven sizing is a problem that can result in paper with inconsistent water resistance. This can be due to uneven distribution of the AKD in the papermaking system. For example, if the AKD is not well-dispersed in the pulp, some parts of the paper might get more sizing than others.

To solve this, you can use better mixing equipment. Make sure the AKD is thoroughly mixed with the pulp before it goes onto the paper machine. You can also adjust the flow rate of the AKD to ensure a more even distribution.

Cationic Retention And Drainage AidFixing Agent in Papermaking Inkjet Paper

7. Impact on Paper Properties

In some cases, using AKD polymer emulsifier can have an impact on other paper properties. For example, it might affect the strength or brightness of the paper. This can be due to the chemical reactions that occur during the sizing process.

To minimize these effects, you need to optimize the AKD dosage and the papermaking conditions. You can also use other additives to counteract any negative impacts. For example, if the AKD is reducing the brightness of the paper, you can use a Fixing Agent in Papermaking Inkjet Paper to improve the optical properties.

Conclusion

In conclusion, while AKD polymer emulsifier is a great product for papermaking, it does come with its fair share of problems. But with the right approach, these problems can be easily solved. By paying attention to dosage, pH, foam, deposits, compatibility, storage, and other factors, you can ensure that you get the best results from our AKD polymer emulsifier.

If you're facing any of these problems or have any questions about using our AKD polymer emulsifier, don't hesitate to reach out to us. We're here to help you optimize your papermaking process and get the most out of our products. Whether you need more information, technical support, or want to discuss a potential purchase, we're just a message away. Let's work together to make your papermaking operations more efficient and successful.

References

  • Papermaking Chemicals Handbook
  • Journal of Pulp and Paper Science